Tribological properties of in-situ synthesized Cr7C3-reinforced Ni-Cr-based coatings fabricated via laser cladding

Abstract

To overcome the inherent limitation of poor tribological properties in ex-situ prepared coatings, resulting from hard-phase decarburization and inferior interfacial bonding, in situ Cr7C3-reinforced Ni-Cr-based composite coatings were successfully fabricated via laser cladding. The influence of the Cr/C molar ratio on the microstructure and hardness of the coatings, as well as their tribological behavior across a wide temperature range, was systematically investigated. The results indicate that the in situ synthesized Cr7C3 strengthening phase exhibits uniform equiaxed features with a Cr/C ratio of 3:1, yielding a microhardness of 1066 HV. At room temperature, the primary mechanism is mild abrasive wear, with a coefficient of friction and a wear rate as low as 0.39 and 1.17 & times; 10- 6 mm3 /(N center dot m), respectively. At elevated temperatures, the tribological performance of the coating exhibits a non-linear trend, and the wear mechanism shifts to a synergistic combination of oxidative, abrasive, and adhesive wear. At 300 degrees C, matrix softening leads to intensified abrasive and adhesive wear, causing an increase in the coefficient of friction (0.60) and the wear rate (6.20 & times;10- 5 mm3/(N center dot m)). However, between 600 degrees C and 900 degrees C, the coefficient of friction drops to 0.43-0.53, and the wear rate stabilizes at approximately 4.20 & times; 10-5 mm3/(N center dot m). This is due to the tribo-oxides layer formed on the worn surface.

Keywords Plus: TEMPERATURE,MICROSTRUCTURE,OXIDATION

Published in TRIBOLOGY INTERNATIONAL,Volume227;10.1016/j.triboint.2026.112807,MAR 2027

Copyright © Lanzhou Institute of Chemical Physics, Chinese Academy of Sciences
Address: No. 18, Tianshui Middle Road, Lanzhou City, Gansu Province, China. Postcode P.C. : 730000 Tel: 86-0931-4968009 Fax: 86-0931-4968019
E-mail: webeditor@licp.cas.cn